All Products

201 Stainless Steel Coil
201 stainless steel is the steel that is resistant to the corrosion of weak media such as atmosphere, steam and water, while acid resistant steel refers to the steel that is resistant to the corrosion of chemical corrosive media such as acid, alkali and salt.
Inquiry Now →

PRODUCT DESCRIPTION


201 Stainless Steel Coil Description

201 stainless steel coil is composed primarily of iron with around 18% chromium and less than 0.15% carbon. It also includes small amounts of manganese, nickel, silicon, nitrogen, and copper. It has higher formability than the 300 series grades. Moreover, it can be hardened by cold working processes but cannot be heat-treated like 304 or 316 grades. 201 is a high manganese and low nickel stainless steel with low nickel content and corrosion resistance. It is widely used in various tabletops, countertops, kitchenware, outdoor decoration engineering, urban decoration industry and low-grade household products. It is also used in medical instruments and automotive parts that require flexibility while maintaining strength under pressure.

Product Parameters

Product Name201 Stainless Steel Coil
TypeSteel Coil
Thickness2.5mm-10.0mm
Length2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc.
Width610mm-2000mm
StandardASTM, AISI, JIS, GB, DIN, EN, etc.
SurfaceBA, 2B, NO.1, NO.4, 4K, HL, 8K, etc.
Scope of Application

Widely used in high temperature and electrical industry, medical equipment construction, chemical, food industry, agriculture and ship parts, food and beverage packaging,

Kitchen supplies, trains, airplanes, conveyor belts, vehicles, bolts, nuts, springs and screens, etc.

CertificateISO, SGS, BV, etc.
Production TechnologyHot Rolling, Cold Rolling
Edge ProcessingEdging, Trimming

Chemical Composition

CSiMnCrNiSP
≤ 0.15≤ 0.755.50~7.5016.00~18.003.50~5.50≤ 0.03≤ 0.06

Mechanical Properties

Tensile Strength Kb (MPa)Yield Strength σ0.2 (MPa)Elongation D5 (%)Hardness
≥ 520≥ 27555-60≤183HB;≤ 100 HRB

Physical Performance

Density(g/cm³)Modulus of Elasticity(Gpa)Coefficient of Thermal Expansion(10-6/°C)Coefficient of Thermal Conductivity(W/m*K)Resistivity(μohm.in)
7.819715.716.227

Surface Selection1745571644774317357941321728.png

PRODUCT DISPLAY

1.png

CUSTOMER CASE

CUSTOMER PRAISE

55.jpg

INQUIRY

Submit

RELATED PRODUCTS